A snag may pull a yarn out of position; a broken yarn interrupts the fabric structure, while a hole leaves an opening that can affect both appearance and strength. These defects are not interchangeable, so record what is actually present before deciding whether a roll can be repaired, downgraded or rejected. The first priority is to identify the affected roll and keep the damaged area out of cutting until it has been assessed.
Possible causes
- Yarn weakness or damage before weaving.
- Machine-related problems, damaged components, or interrupted yarns.
- Rough handling, sharp surfaces, or improper roll movement.
- Finishing and inspection equipment that catches the fabric.
- Packaging or storage damage after inspection.
Inspection procedure
- Record the style, color, lot, roll number, and defect location.
- Describe the defect consistently and photograph it with a scale or clear reference.
- Inspect nearby fabric to determine whether the defect is isolated or recurring.
- Mark and segregate affected rolls or sections according to the inspection procedure.
- Report defect frequency and affected length to the responsible quality team.
Preventing repeat defects
Review yarn quality, weaving and finishing records, machine maintenance, handling, and packing. Establish an agreed inspection standard and defect classification with the buyer. Repair, downgrade, or reject decisions depend on the agreed quality standard and defect location; do not assume every defect can be safely repaired.
Before shipment
Keep inspection records linked to roll identification and ensure the shipment matches the approved quality criteria. For critical programs, agree the inspection method and acceptance limits before production begins.
Share the fabric type, construction, intended use, quantity, and required inspection standard through our contact page.
Classify the defect and map its frequency
Record whether the issue is a surface snag, a broken yarn, a hole or damage created during handling. Note the fabric face, direction, size and distance from the selvedge, then map findings by roll position. A repeated defect at similar intervals can point to equipment contact, while scattered damage may have another cause; the pattern is useful evidence but does not prove the source by itself.
Retain a marked sample and identify the roll and lot before cutting. Review handling, storage and machine contact points with the production team. Where a defect affects garment appearance or strength, agree how the affected area will be identified and removed, and what evidence is needed to accept the remaining fabric. Reinspect after corrective action and record the disposition for each roll.